Filaflex Conductive

QUESTION #1

"Do I have to use a hardened nozzle on my printer to print Filaflex Conductive?"

NO, it is not necessary. You can print with whatever nozzle you have without a problem, but if you print a lot with this material, we advise you to use a hardened nozzle to avoid wear.

Hardened Nozzle

QUESTION #2

"Is it safe to print with Filaflex Conductive filament or can it end up damaging my printer?"

Yes, it is totally safe and will not damage your printer, but to keep it in good condition we recommend that you clean the nozzle very well when you finish printing with this filament. This way you will remove any sediment that may have remained in the hotend. You can use another material such as PET-G to clean the nozzle.

Nozzle Cleaning

QUESTION #3

"What material is added to make the filament conductive?"

We use a special formulation containing lamp black, which makes the TPU filament conductive.

Conductive Material

QUESTION #4

"Does Filaflex Conductive lose its flexibility after printing?"

Not at all. Filaflex Conductive does not lose its elasticity after printing. The finish of this material is a flexible and electrically conductive part. Its mechanical and conductive properties remain intact.

Flexibility Test

QUESTION #5

"What is the Shore hardness of Filaflex Conductive filament?"

It has a 92A Shore hardness, which makes it compatible to be printed on most printers, even bowden type extrusion printers.

Shore Hardness

QUESTION #6

"What resistance does the conductive filament present?"

To learn about the resistivity of Conductive Filaflex (also known as specific resistance), we recommend consulting with our team. In order to determine if the material will fulfill the functions in a specific project, it's important to note that the resistance changes depending on its printing.

Resistance Testing

QUESTION #7

"What can I do if I have adhesion problems between layers?"

Being a material with high carbon loading, heat dissipates very fast and therefore the adhesion of the part may be weakened depending on its geometry. The best solution is to adjust the printing parameters. Print at a slow speed, between 20-25 mm/s, and at high temperature, between 240-255ºC, eliminating the layer fan in all layers, to avoid heat dissipation being too fast.

Layer Adhesion

Find out how Filaflex Conductive works

See More Applications of Filaflex Conductive

Prev post
Next post

Thanks for subscribing!

This email has been registered!

Shop the look

Choose options

Recreus
Edit option
Back In Stock Notification

Choose options

this is just a warning
Login